Paint Problem Solver

Identify and resolve common automotive paint defects. Expand each problem below to learn about its causes, how to repair it, and how to prevent it in the future.

Air EntrapmentCraters: Small crater-like openings in or on the paint film+

Cause

Trapped or buried air pockets in the wet paint film that rise to the surface and "burst" causing small craters. Lack of atomization may be due to one or more of the following:

Repair

Sand with 1200 or finer grit sandpaper, then compound and polish to restore gloss.

Or, sand smooth and refinish.

Prevention

Note: Some cases of air entrapment may appear very similar to solvent pop or dust contamination. Air entrapment normally occurs when the film is still wet and can be removed with compounding. Solvent pop will appear after the film is "skinned over" and when sanded will have pinholes. Dust contamination will appear while the film is drying but still "tacky"; these craters will have a speck of dirt in the center.

BleedingDiscoloration: A red or yellow discoloration in the topcoat color+

Cause

Solvent in the new topcoat dissolves soluble dyes or pigments in the original finish, allowing them to seep into and discolor the new topcoat.

Repair

Allow color to cure, isolate with two component undercoat(s) and refinish.

Or, remove original paint film and refinish.

Prevention

Isolate suspected bleeding finish by applying a two component surfacer and/or sealer. Allow to cure following product recommendations, then apply desired topcoat.

BlisteringPimples, Bubbles, Bumps: Swelled areas appearing as pimples or bubbles in the topcoat film+

Cause

Moisture trapped beneath the paint film due to:

Repair

Remove affected area and refinish.

Extreme cases must be stripped to bare substrate before refinishing.

Prevention

BlushingCloudy, Milky: A milky gray cloud appears on the surface shortly after application+

Cause

When spraying in humid conditions, air from the spray gun and solvent evaporation lowers the substrate temperature below the dew point, causing moisture to condense in or on the paint film. Aggravated by too fast drying or unbalanced thinner/reducer.

Repair

Should blushing occur during application:

If the finish has dried, minor blushing may be corrected by compounding or polishing. Severe blushing will require sanding and refinishing.

Prevention

ChalkingOxidizing, Fading, Weathering: A chalky white appearance on the surface of the paint film+

Cause

Pigment is no longer held and protected by resin, resulting in a powder-like surface and lack of gloss due to:

Repair

Compound to remove oxidation and polish to restore gloss.

Or, sand to remove "weathered" paint film and refinish.

Prevention

Chemical Staining / EtchingSpotting, Discoloration, Acid Rain: Irregular shaped pitting, etching or discoloration+

Cause

A chemical change occurs when harmful environmental contaminants (such as acid rain, tree sap, bird droppings, road tar, etc.) remain on the surface for an extended period of time.

Repair

Prevention

\* When sanding and buffing a basecoat/clearcoat finish, a minimum clearcoat film thickness of 2 mils is required to maintain adequate UV protection. If correcting the damage will remove more than 0.5 mils, refinishing is recommended.

ChippingStone Chips, Nicks, Bruises: Small areas of damage leaving a nick, notch or void in the finish+

Cause

Loss of adhesion of the paint film to the substrate caused by an impact from stones or other hard objects.

Repair

Sand and featheredge damaged areas to remove chips, then refinish.

Prevention

Color MismatchMis-Tint, Off-Color/Shade: Noticeable difference in color between original and repair+

Cause

Repair

If color is close enough to blend:

If color must be tinted:

Prevention

CrackingChecking, Splitting, Crazing, Crowsfeet: Cracks or lines of various lengths and widths in the topcoat+

Cause

Repair

Remove all cracked paint film and refinish.

Prevention

Dust ContaminationDirt or Dust in Finish: Foreign particles embedded in paint film+

Cause

Repair

Prevention

Note: Fine dust particles that fall on a tacky surface can be encapsulated by the finish, creating an appearance almost identical to solvent pop. This usually occurs on vehicles removed from the booth in a tacky condition. Fine dust contamination can be removed by sanding and polishing. If the condition is solvent pop, the finish will contain pinholes or small craters after sanding.

Edge MappingFeatheredge Lifting, Edge Ringing: Raised or lifted edges outlining sand-throughs or featheredges+

Cause

Solvent from the new topcoat penetrates a solvent-sensitive substrate causing lifting or wrinkling that outlines the featheredge.

Repair

Prevention

FisheyesSilicone Contamination, Cratering: Small circular, crater-like openings during or after spray application+

Cause

Repair

Prevention

LiftingRaising, Shriveling, Swelling, Wrinkling: Existing paint film shrivels or swells during new finish application+

Cause

Solvents in a newly applied product attack the previous finish due to:

Repair

Remove lifted areas and refinish.

Prevention

Loss of GlossDieback, Matting, Hazing, Dulling: A dulling of the gloss as the film dries or cures+

Cause

Repair

Allow finish to cure thoroughly, compound or polish to restore gloss.

Or, sand and refinish.

Prevention

MottlingStreaking, Tiger Stripes, Floating: A streaked, spotty or striped appearance in metallic color+

Cause

Uneven distribution of metallic flake caused by:

Repair

Caution: Large areas of basecoat must have clearcoat applied before sanding. Small nibs may be removed from basecoat by wet sanding on the defect only. Apply additional basecoat to the sanded area before clearcoating.

Prevention

Orange PeelTexture, Lack of Flow: Paint film with an uneven texture resembling the skin of an orange+

Cause

Repair

Prevention

PeelingDelamination: Loss of adhesion or separation of the paint film from the substrate+

Cause

Repair

Remove the finish in the affected area, featheredge, and refinish.

Or, strip to bare substrate and refinish.

Prevention

Pinholes in Body FillerBubbles, Bondo Pits: Small holes or bubbles in or on top of putties or body fillers+

Cause

Air or gas bubbles become trapped inside putty or filler during mixing or application, exposed during sanding. Air or gas is trapped when:

Repair

Apply a thin layer of polyester glazing putty (properly catalyzed and mixed), sand smooth and continue the repair process.

Prevention

Rail DustSmall rust-colored bumps or specks in the surface of the paint film+

Cause

When vehicles are transported by rail, iron dust particles created by friction between train wheels and the track settle on the finish. When exposed to oxygen and moisture, this dust corrodes and becomes embedded in the finish.

Repair

Prevention

Unfortunately, since this type of damage usually occurs during shipment or storage, little can be done to prevent its occurrence.

Runs / SagsCurtains, Hangers: Coatings that fail to adhere uniformly, causing beads, droplets, or slippage+

Cause

Repair

Prevention

Sanding Marks / ScratchesDark and/or streaked marks resembling sand scratches in the paint film+

Cause

Scratching or distorting metallic/mica flakes close to the surface of the paint film due to:

Repair

Allow finish to dry, sand and refinish.

Prevention

SandscratchesSwelling, Sinking: Visible lines or marks in the paint film following the direction of sanding+

Cause

Repair

Allow finish to dry/cure, sand smooth, compound or polish to restore gloss.

Or, sand and refinish.

Prevention

\* For best results, use the premium two component undercoat system.

SeedinessGrainy, Speckled, Gritty, Dirty: Solid particles of various shapes embedded throughout the paint film+

Cause

Repair

Remove the wet paint film with solvent, clean and refinish.

Or, sand smooth and refinish.

Prevention

ShrinkageRinging, Edge Mapping, Bullseyes: Repaired area or featheredge becomes visible hours, days or weeks after repair+

Cause

Repair

Allow the affected area to thoroughly dry/cure, sand and refinish.

If additional filling is necessary, apply a primer surfacer, sand smooth and refinish.

Prevention

Soft FilmSoft Finish, Soft Coat: The paint film is soft to the touch and will fingerprint or waterspot+

Cause

Repair

Prevention

Solvent PoppingGassing, Popping: Small bubbles, pinholes or crater-like openings in or on the paint film+

Cause

Liquid solvent becomes "trapped" in the paint film when the surface layer skins over too quickly, preventing evaporation. Solvents can be trapped due to:

Repair

Allow finish to thoroughly dry/cure, sand smooth and refinish. Inspect carefully to ensure all craters have been removed.

Severe popping will require removal of the affected film. Prime, seal and recoat as necessary.

Prevention

Note: Fine dust particles that fall on a tacky surface can create an appearance almost identical to solvent pop. This usually occurs on vehicles removed from the booth in a somewhat tacky condition. Fine dust contamination can be removed by sanding and polishing. If the condition is solvent pop, the finish will contain pinholes or small craters after being sanded.

Staining / Plastic Bleed ThroughDiscolored, Bleed-Back: Yellow-brown discoloration over areas repaired with polyester body filler+

Cause

Repair

Allow topcoat to thoroughly cure.

Sand affected area, isolate with two component undercoats and refinish.

Prevention

Tape TrackingTape Marks/Tracks: An imprinted line or texture in the dried paint film from masking tape+

Cause

Finish not dry before taping, causing solvent entrapment between finish and tape.

Using a non-automotive tape for multi-color finishes; solvents from additional color soak through the tape into the previous color.

Repair

Prevention

TransparencyTransparent, Poor Hiding, Translucent: The original finish or undercoat is visible through the topcoat+

Cause

Repair

Apply additional coats of color until hiding is achieved.

Or, sand and apply similar colored undercoat/ground coat and refinish.

Prevention

Note: Spray monitors (hiding power labels, opacity charts) provide a contrasting feature to observe hiding power during spray application. When black and white can no longer be seen through the color, complete coverage is achieved.

Water SpottingCircles with raised edges or whitish spots resembling the shapes of water droplets+

Cause

Allowing water to come into contact with a finish that is not thoroughly dried/cured.

Washing finish in direct sunlight.

Repair

Prevention

WrinklingShriveling, Crinkling: The surface contains irregular grooves or ridges resembling the skin of a prune+

Cause

Repair

If defects are minor: Sand the top surface smooth, allow to cure and refinish.

If defects are severe: Remove the affected area and refinish.

Prevention

Need help? Call (858) 909-2110 or email support@tcpglobal.com for additional support from our team.

Scroll to page top

shop.app

shop.app is blocked

This page has been blocked by an extension

ERR_BLOCKED_BY_CLIENT

Reload

This page has been blocked by an extension

tcpglobal.com

tcpglobal.com is blocked

This page has been blocked by an extension

ERR_BLOCKED_BY_CLIENT

Reload

This page has been blocked by an extension

Leave us a message

There are no agents available right now.

Please select an option * Order IssueProduct InquiryReturnsShipping Questionz-Other

I consent to the website cookie policy.

Send

Thank you!

We have received your message and will get back to you as soon as possible.

Dismiss

Message not sent

Contact form is not available

Dismiss

Sending...

Cancel Yes